Re: [MW:17524] Effect of grain growth in toughness and Softness of a metal

For more details, please refer to:
http://www.osti.gov/bridge/purl.cover.jsp?purl=/861397-tb7pb9/86139.

--- On Mon, 22/4/13, Shomenath Bagchi <snbagchi@ymail.com> wrote:

From: Shomenath Bagchi <snbagchi@ymail.com>
Subject: Re: [MW:17511] Effect of grain growth in toughness and Softness of a metal
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Monday, 22 April, 2013, 9:36 PM

Grain growth makes a softer and inferior structure in most cases and is avoided. It also reduces hardness but may increase ductility in a few cases,
at the cost of tensile strength reduction. You may consult heat treatment theories from internet for explanation.



From: Binoy Soman <binoy.spp@DAELIM.CO.KR>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, April 22, 2013 3:48 PM
Subject: [MW:17506] Effect of grain growth in toughness and Softness of a metal

 
Dear experts,
 
Kindly explain the relation between grain growth, toughness, hardness & ductility. If anybody have some texts which explains the basic changes that happens during heat treatment, please share.
 
S.binoy
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...