RE: [MW:17522] Effect of grain growth in toughness and Softness of a metal

Dear sir,

 

Grain structure are largely affecting on the hardness & toughness.

 

Fine grade structure that are receiving by (controlled temp cooling)annealing or furnace cooling will give good toughness, ductility & impact values.

Course grain structure are receiving by rapid cooling will give high hardness.

 

You can refer an IRON CARBIDE DIAGRAM to see CCT diagram for more knowledge on phase transformation & structure behaviour.

 

Regards

 

Dinesh

@Latur

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vasanth 19
Sent: Monday, April 22, 2013 4:45 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:17515] Effect of grain growth in toughness and Softness of a metal

 

Hi Binoy,

 

    As I know grain size increases, hardness will increase, therefore toughness and ductility will decrease..

 

 

Thanks,

 

P.Vasanth

+91-9840466402

+91-7667116860

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...