Monday, April 22, 2013

Re: [MW:17516] Welder validity

Dear sir,

kindly follow QW-300.3(page no.-54) and QW-322(page no.-56) of ASME SEC-IX only.

Thanks & Regards
hemal chauhan
Engineers india limited.


From: HAREESH K V <hareesh13h@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Monday, 22 April 2013 10:50 AM
Subject: Re: [MW:17502] Welder validity

Now as the manufacturer is same there is no need of re qualification, because the welder is welded under the quality guidelines of the manufacturer not the contractor X or Y.

Please refer QW 300.2 (a) of ASME BPVC Sec IX.

Now if the manufacturer itself is working under the quality guidelines of different clients, then the welder has to be re-qualified.

Hope for comments if i am wrong, with references.


On Sun, Apr 21, 2013 at 4:49 PM, Nirmal kumar Mondal <nkmp.mondal@gmail.com> wrote:
he need again to qualified as a new employer.


On Sun, Apr 21, 2013 at 3:39 PM, Prakash Hegde <pb.hegde@yahoo.com> wrote:
He need requalification as his employer is cahnged so his Identification is changed
Regards
 
Hegde

--- On Sat, 20/4/13, Maulik Thakkar <mlkthakkar2@gmail.com> wrote:

From: Maulik Thakkar <mlkthakkar2@gmail.com>
Subject: [MW:17489] Welder validity
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, 20 April, 2013, 9:25 PM

Dear all,
Query- one qualified welder under x contractor at one manufacturer. Now consider he left the x contractor & join y contractor & working under same manufacturer but at different location.
In view of above case is he qualified to do welding under y contractor at same manufacturer located at different place?......or need requalification?
Regards,
MHT
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
----------------------
Hareesh K V
+91-9447625012


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...