Monday, April 22, 2013

Re: [MW:17504] how to make material data report (MDR)

Hi, MDR means Manufacturers Data Report/Record. There is no standard norm as such and many a times the clients require what should be the contents in the MDR/MDB (Book). However in general you can have the following for compiliation.
Table of Contents and indexes will be as follows
Final Release Note
Inspection Test Plan (ITP)
WPS and PQR
Welders Master List
Welders Performance Qualification
Material Test Certificates
Consumable Test Certificates
Welding Log
Materials and Welding Traceability Report/Record/Log (Weld Map)
NDT Procedures
NDT Personnel Certs
NDT Reports
Dimensional Reports
Hydrostatic Test Report
Heat Treatment Reports
Design and Calculations
Technical Queries
Non Conformances
Miscelleanous.
 

From: Ravindra <drnath.bvil@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 22 April 2013, 12:41
Subject: Re: [MW:17498] how to make material data report (MDR)

Dear mach.....

I guess MDR means Manufacturers Data Report. Correct me if I am wrong.


On Sun, Apr 21, 2013 at 8:20 AM, Maput Gani <aku.maput@gmail.com> wrote:
Dear Expert,

wondering, how to make material data report (mdr), or any one could share to me example mdr templates, procedure etc?



thanks in advanced

machfud
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to mailto:materials-welding%2Bunsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
With Regards,

D.R
.
Nath,



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...