sir
   according to asme sec 9 ,article -3, qw-300.2(d) is as follow
 

(d) The Code recognizes that manufacturers or contractors
may maintain effective operational control of Welder/
Welding Operator Performance Qualification (WPQ) records
under different ownership than existed during the
original welder or welding operator qualification. When a
manufacturer or contractor or part of a manufacturer or
contractor is acquired by a new owner(s), the WPQs may
be used by the new owner(s) without requalification, provided
all of the following are met:
(1) the new owner(s) takes responsibility for the
WPQs
(2) the WPQs reflect the name of the new owner(s)
(3) the Quality Control System/Quality Assurance
Program reflects the source of the WPQs as being from
the former manufacturer or contractor,
 
so means no need any further qualification only need to verify manufacturer quality control manual for this issue ,they have allowed the welder to weld in this condition , if ok , the welder have to submit his WPQT+UPDATED CONTINUITY RECORD SIGNED BY HIS SUPERVISOR
 
Thanks & best regards.
Mohammad Jawed Anwar .
(welding inspector)
Mob no #  +966569799776.


On Sun, Apr 21, 2013 at 2:19 PM, Nirmal kumar Mondal <nkmp.mondal@gmail.com> wrote:
he need again to qualified as a new employer.


On Sun, Apr 21, 2013 at 3:39 PM, Prakash Hegde <pb.hegde@yahoo.com> wrote:
He need requalification as his employer is cahnged so his Identification is changed
Regards
 
Hegde

--- On Sat, 20/4/13, Maulik Thakkar <mlkthakkar2@gmail.com> wrote:

From: Maulik Thakkar <mlkthakkar2@gmail.com>
Subject: [MW:17489] Welder validity
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, 20 April, 2013, 9:25 PM

Dear all,
Query- one qualified welder under x contractor at one manufacturer. Now consider he left the x contractor & join y contractor & working under same manufacturer but at different location.
In view of above case is he qualified to do welding under y contractor at same manufacturer located at different place?......or need requalification?
Regards,
MHT
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...