Re: [MW:17498] Re: Radiography aerospace M250 welds

Sir,

Fabricator feels that as 10ISO16 wire is seen in both the films, will we miss a defect more than this size in D4. As you have suggested we are consulting the designer and working out options without repair.

Regards

Mohan

On Sat, 20 Apr 2013 01:08:26 -0700 (PDT), SV Swamy wrote
> If I remember right D2 is a slower finer grained film. Thus it may show some fine indications missed by D4. You can switch to D2 but you may find such indications and would have a problem deciding whether to leave them alone (and monitor them later in service if possible) or repair them. Repair may sometimes worsen and introduce more discontinuities. 
>
> Better discuss with designer if possible before switching. 
>
> Swamy
> Retd. QA Metallurgist
> Nuclear Fuel Complex, Hyderabad
>
> On Friday, April 19, 2013 12:10:35 PM UTC+5:30, Mohanananthanarayanan KR wrote:
Dear all,
>
> As per specification we have D4 film to be used for radiography of 7.8mm welds
> of M250.As an investigation of a defect in UT D2 film was used and it detected
> faint indications. The sensitivity IQI is seen in both the films as per
> specification. Should we change to D2 film?
>
> Regards
>
> Ananthanarayanan
> Trivandrum
>
> **Print this e-mail only if absolutely necessary. Save paper and keep India Green**
>
> ***The information contained in this e-mail message and / or attachments to it may contain confidential or privileged information. If you are not the intended recipient and received this e-mail in error, please notify us by reply e-mail / telephone and  delete the message and attachments permanently. Thank you.***
>
>

> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>  
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>  
>  


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...