If your weldor is qualifying per ASME Section IX, then the use of alternate base metals is discussed in QW-423.1.  The combination you state below is permissible and weldor is qualified. 

 

According to retired committee member I know, the rational is that weldor is only trying to show the ability to deposit sound weld metal.  The previously performed PQR established that the actual base metal-weld metal combination possessed the required metallurgical properties.  Therefore, the only important issue is that the base metal be sufficiently compatible with the filler metal to allow the weldor qualification coupon to be tested.  

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of ali.himayat@gmail.com
Sent: Monday, April 29, 2013 11:31 AM
To: materials-welding@googlegroups.com
Subject: [MW:17592] welder is valid

 

whether welder is valid if WQT done on P1 to P1 with ER308 (F6 A5.9), autual welding production WPS is P8-P8 with filler rod ER308.

Please answer.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...