Saturday, April 27, 2013

[MW:17571] Brass to CS joining process

Respected all,

I need guidance on the joining process between Brass and CS.

Situation:
One side is valve (TBE IS778 brass-female threaded) and the other side is threaded pipe (SA106 GR-B-male threaded).

Requirement: Seal welding only.

Service: Drinking Water.

(If any more details are needed please revert back)

Question is:

1) What is the joining process to be followed.
2) Consumable to be used.
3) If procedure is available please share it.
4) Qualification procedure to be followed.

Thanks in advance,

--
----------------------
Hareesh K V
+91-9447625012


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...