What is the test pressure ?
Better to remove the paint completely and You can use either neoprene or PTFE gaskets.
Praphulla
Sent from my iPhone
On 28-Feb-2013, at 14:05, Lalu r p <lalucpt@gmail.com> wrote:
> Dear sir
> Normally for flange faces we do not paint the surface to ensure the
> proper sealing.and it is normally machined for the gasket tightness.
>
> On 2/28/13, G Sreenivas Rao <gsrinivasg3@gmail.com> wrote:
>> Dear sir
>> In pressure vessel flat flange shall not be painted, this is for
>> gasket seating and if painted the are will not be giving seal
>> tightness. please ensure if the area is giving seal tightness then can
>> be left as it is.
>>
>> Regards
>> G.Sreenivas Rao
>>
>> On Wed, Feb 27, 2013 at 12:26 PM, Suresh Babu <suresh75.babu@gmail.com>
>> wrote:
>>> Dear Experts,
>>>
>>> We have some flat face flanges in Pressure vessel. The pressure vessel
>>> manufacturer done the painting on the flat face up to the bolt hole and
>>> left
>>> the remaining face unpainted. I hope the entire flat face will leave as
>>> unpainted. I am trying to get info from client which type of Gasket they
>>> will use at site.
>>>
>>> Please put your suggestions.
>>>
>>> --
>>> Best Regards,
>>> Suresh Babu,
>>> suresh75.babu@gmail.com
>>>
>>> --
>>> To post to this group, send email to materials-welding@googlegroups.com
>>> To unsubscribe from this group, send email to
>>> materials-welding+unsubscribe@googlegroups.com
>>> For more options, visit this group's bolg at
>>> http://materials-welding.blogspot.com/
>>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>>
>>> The views expressed/exchnaged in this group are members personel views
>>> and
>>> meant for educational purposes only, Users must take their own decisions
>>> w.r.t. applicable code/standard/contract documents.
>>> ---
>>> You received this message because you are subscribed to the Google Groups
>>> "Materials & Welding" group.
>>> To unsubscribe from this group and stop receiving emails from it, send an
>>> email to materials-welding+unsubscribe@googlegroups.com.
>>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Better to remove the paint completely and You can use either neoprene or PTFE gaskets.
Praphulla
Sent from my iPhone
On 28-Feb-2013, at 14:05, Lalu r p <lalucpt@gmail.com> wrote:
> Dear sir
> Normally for flange faces we do not paint the surface to ensure the
> proper sealing.and it is normally machined for the gasket tightness.
>
> On 2/28/13, G Sreenivas Rao <gsrinivasg3@gmail.com> wrote:
>> Dear sir
>> In pressure vessel flat flange shall not be painted, this is for
>> gasket seating and if painted the are will not be giving seal
>> tightness. please ensure if the area is giving seal tightness then can
>> be left as it is.
>>
>> Regards
>> G.Sreenivas Rao
>>
>> On Wed, Feb 27, 2013 at 12:26 PM, Suresh Babu <suresh75.babu@gmail.com>
>> wrote:
>>> Dear Experts,
>>>
>>> We have some flat face flanges in Pressure vessel. The pressure vessel
>>> manufacturer done the painting on the flat face up to the bolt hole and
>>> left
>>> the remaining face unpainted. I hope the entire flat face will leave as
>>> unpainted. I am trying to get info from client which type of Gasket they
>>> will use at site.
>>>
>>> Please put your suggestions.
>>>
>>> --
>>> Best Regards,
>>> Suresh Babu,
>>> suresh75.babu@gmail.com
>>>
>>> --
>>> To post to this group, send email to materials-welding@googlegroups.com
>>> To unsubscribe from this group, send email to
>>> materials-welding+unsubscribe@googlegroups.com
>>> For more options, visit this group's bolg at
>>> http://materials-welding.blogspot.com/
>>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>>
>>> The views expressed/exchnaged in this group are members personel views
>>> and
>>> meant for educational purposes only, Users must take their own decisions
>>> w.r.t. applicable code/standard/contract documents.
>>> ---
>>> You received this message because you are subscribed to the Google Groups
>>> "Materials & Welding" group.
>>> To unsubscribe from this group and stop receiving emails from it, send an
>>> email to materials-welding+unsubscribe@googlegroups.com.
>>> For more options, visit https://groups.google.com/groups/opt_out.
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> For more options, visit https://groups.google.com/groups/opt_out.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments