Dear sir
In pressure vessel flat flange shall not be painted, this is for
gasket seating and if painted the are will not be giving seal
tightness. please ensure if the area is giving seal tightness then can
be left as it is.

Regards
G.Sreenivas Rao

On Wed, Feb 27, 2013 at 12:26 PM, Suresh Babu <suresh75.babu@gmail.com> wrote:
> Dear Experts,
>
> We have some flat face flanges in Pressure vessel. The pressure vessel
> manufacturer done the painting on the flat face up to the bolt hole and left
> the remaining face unpainted. I hope the entire flat face will leave as
> unpainted. I am trying to get info from client which type of Gasket they
> will use at site.
>
> Please put your suggestions.
>
> --
> Best Regards,
> Suresh Babu,
> suresh75.babu@gmail.com
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...