Tuesday, February 26, 2013

Re: [MW:16872] Rt review

Dear Abhilash.
My opinion is to identify the easiest way while RT film interpretation, Tungsten inclusion defect can be seen root weld , & Cap weld.

Regards
N.David 

On Sun, Feb 24, 2013 at 1:10 AM, abhilash <abhilash.jaa@gmail.com> wrote:

Dear experts:

                         I need to know that during the review of rt film is it possible to identify two diffrent process.ie root by tig upto fill up smaw and then again capping is done by tig .







--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 



--
N.Devan
Senior Welding Inspector-AWS
Chennai -INDIA
0091 9840330143

 YASREF
PQMD Quality Division
K.S.A  Yanbu
+966504534524
Natrajan.Devan@yasref.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...