Re: [MW:16858] Fluid Category M as per B 31.3


What is the process you are dealing with...?
If you are dealing with gas treating plants, sour gas is always a category M fluid.
In oil & gas processes wherever the fluid contains more than certain amounts of H2S, it makes it a category M fluid too.

Regards
Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
  


On Sun, Feb 24, 2013 at 9:17 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
Refer Chapter VIII and Appendix M, it has to be categorised by Owner. 

examples can be toxic gas like, methyl isocyanate (remember Bhopal Gas leak incident)

On Sat, Feb 23, 2013 at 7:22 PM, Saravanan Murugappan <saravananmurugappan@gmail.com> wrote:
Gents,
 
1.Plz Advice how to find out  fluid category M?
 
2.Is there any particluar service we can say easily as Category M?
 
 
 
 


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...