[MW:16744] UC beam concavity

Dear sir,

 

please find attached photos for your reference,with raw material defects.This beams are UC 356*368*153 IN Section are  flange concavity 4 mm.Please confirm can anybody tell me whats an acceptance criteria for concavity AS per EN10034.We check in standard but it’s not clearly mentioned about acceptance limit.

 

current status : material under hold / clarification

 

waiting for your reply.

 

thanks & regards

 

dinesh

 

dubai

 