[MW:16656] Required PQR Test Help

Dear Experts,

Our company is going to make a new PQR and WPS but since I am new at ASME sec IX and B31.3, I would like to verify my tests before doing them.

So PQR specs are;

Thickness                              10mm (WPS qual. 10-15mm)

Mat                                        Plate - SA516 Gr60 & SA516 Gr70 (this will qualify bot P1G1 and P1G2 mats right?)

Preheat                                  38°C Min(client spec)

Interpass Temp                       250°C Max

PWHT                                   620°C (120min, 100°C/hr)

Pos                                       3G

Type                                      GTAW + SMAW

 

Tests:

2              Tensile Test

2              Face Bend Test

2              Root Bend Test

4              Side Bend Test (Do we need this?)

5?           Toughness Test (Charpy V-Noch at -46 C is enough?)

Hardness

Radiography


And the other thing is how big test coupon should I weld to get these tests.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...