RE: [MW:15426] CAN WE USE IS 1367 GR. 10.9 INSTEAD OF A 193 GR. B7

yes, get approval from purchaser


Thank & Best Regards,

 

M Veera SAMY- Bureau Veritas.

Coimbatore

 

 


 

From: hsuthar@chemithon.co.in
To: materials-welding@googlegroups.com
Subject: [MW:15425] CAN WE USE IS 1367 GR. 10.9 INSTEAD OF A 193 GR. B7
Date: Sat, 29 Sep 2012 14:04:20 +0530

Dear pls reply me can we use bolt for IS 1367 GR. 10.9 INSTEAD OF A 193 GR. B7.

Pls reply with reason

 

HEMANT SUTHAR

QA/QC

CEPL-SILVASSA

9712973092

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...