Re: [MW:15398] Impact test requirement as per ASME SEC VIII Div I

Also check SA 370 Table 9

On Wed, Sep 26, 2012 at 8:55 AM, duc hoang <hoangvanduc79@gmail.com> wrote:
Dear Mano

Please see UG-84(g)(5)

Regards
Dc

2012/9/25 manoj john <manojacgnr@gmail.com>
Dear Mr.Raj

Thanks for reply, and what will be the acceptable value at these temperature.

With Regards.
Mano

On Sun, Sep 23, 2012 at 6:51 PM, RAJASEKARAN <nrajasek@velosi.com> wrote:

(1)       -49 C for (10x5), -46 C for (10x6) – Table UG 84.2

(2)       No

 

Raj

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of manoj john
Sent: 23 September 2012 12:23
To: materials-welding@googlegroups.com
Subject: [MW:15363] Impact test requirement as per ASME SEC VIII Div I

 

Dear members,

 

I have following points to be clarified, please give your expert advise.

 

1) I have to do Procedure Qualification test as per ASME Sec. IX on a test coupon having 8 mm thk with Impact test at  -38 degree C, after machining the specimen size may be reduced to 10 x 5 x 55 or 10 x 6 x 55, in this case at what temperature I have to do 'V' notch  impact test and what will be the acceptable toughness value  as per ASME SEC VIII Div. I.

 

2) If we do procedure qualification test with impact test on P1 Gr. 2 to P1 Gr. 2  materials can I use this procedure qualification to weld P1 Gr 2 to P1 to Gr. 1 as per ASME Sec. IX.

 

Thanks in advance 

 

Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...