Dear All, 

Air condition room is the best place where we can control the moisture content / humidity.  but the air con should be in good condition & temperature should be controllable, this is specially applicable for low hydrogen electrodes , SAW flux & FCAW consumables .

Kind Regarda,

Sukamal Naskar

Bohler Welding Group Asia Pacific

Sent from my iPhone

On 22 Sep, 2012, at 11:02 PM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:

Dear experts,

Whether welding consumable storage in air-conditioned (AC) room is acceptable,including low hydrogen and SS electrodes. Ex: E9018-B9,E7018-1,E316L etc.,
 
Thanks & Regards,
Naresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...