Re: [MW:15355] API 5LD - Weld OVerlay Pipe, NDE requirements

Dear Mr. Vu Duc Thusn,

QW-453 shows a Nominal Base Metal Thickness Qualified (T ).

My query is :-
1) Whether Single layer weld (Consisits of 4mm) PQR Qualifies for
Double layer.(Consists of 4mm)

With Regards,
Ashish P


On Thu, Sep 20, 2012 at 3:51 PM, vdthuan <dthuan117@gmail.com> wrote:
>
> Dear Ashish P
>
> Your welder is qualified for multi layer base on QW-453 section IX, " T qualified to un limit" and see note 1,
>
>
>
> Best Regards,
>
> Vu Duc Thuan
>
> Phone: +84(0) 983 017 936
>
>
>
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ashish Pathrabe
> Sent: Thursday, September 20, 2012 4:17 PM
> To: materials-welding@googlegroups.com
>
>
> Subject: Re: [MW:15349] API 5LD - Weld OVerlay Pipe, NDE requirements
>
>
>
> Dear Experts:
>
>
>
> Query:-
> a) If WPS & PQR are qualified in INCONEL Overlay in Single Layer (4-5mm) .After machining it will b 3.00 mm
>
> b) Is it Qualified for Multi layer Overlay/Cladding.
>
> PLs , guide with Reference code.
>
> With regards,
> Ashish P
>
> On Mon, Sep 17, 2012 at 11:26 AM, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
>
>
> Please see the answer against the query.
>
>
>
>
> On 15 September 2012 16:54, DOKKU AJAY <akdd83@yahoo.com> wrote:
>
> Dear Experts,
>
>
>
> Kindly go through the below case and the query. Your interpretaion of the requirement of API 5LD will be helpful.
>
>
>
> Case:
>
>
>
> We have to weld overlay on the inside of 36" NPS pipe (7 Mtr Long) with Inconel 625. Minimum 2 layers to be deopisted for final CRA thickness of 3.2mm minimum.
>
>
>
> The Pipe is having a Long seam and is in accordance with API 5L PSL2.
>
>
>
> My Query:
>
>
>
> 1. Whethter these overlayed pipes can be considered as Welded Clad Pipe? If yes, then
>
> A: Pipe will be considered as weld overlayed pipe.
>
>
>
> 2. Whether the radiogrpahy in accordance with Clause 11.1.1 of API 5LD is to be done throughtout the length of the long seam before weld overlay or after weld overlay.
>
>
>
> A: No. Pipe manufacturer performs RT of weld seam. If not done, you have to perform.
>
>
>
> 3. When the 36" NPS pipe is supplied by other vendor with radiogrpahy as per API 5L PSL2 and the weld overlay is done by us on the inside of the pipe, does the clasue 11.2 of API 5LD is applicable in this case.
>
>
>
> A: No
>
>
>
>
>
> 3. What all NDE is applicable in this case.
>
> A : PT shall be performed on each layer of weld verlay (1st Layer & 2nd Layer).
>
>
>
>
> Regards,
>
> Dokku Ajay Kumar
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...