Dear friends,

is it possible to change an E7018-1 electrode to E7018 in a WPS without requalification.
Charpy V notch test value is applicable in this case.
Code is AWSD1.1.
I found in table 4.6 in AWSD1.1 as changing of  electrode  is possible with the same SFA number and F number and A number.
Please advice..........
--
Thank you,
 
Sandeep.k.p
Dubai,UAE
Mob:- +971 557405828

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...