[MW:15414] welding of AISI 9310

Dear experts
I have to manufacture a welding electrode extruder head part for that  AISI 9310 material is recommended.
Element Content (%)
Ni 3.00-3.50
Cr 1.00-1.40
Mn 0.45-0.65
Si 0.15-0.30
P 0.025 (max)
S 0.025 (max)
Mo 0.08-0.15
C 0.08-0.13
the process sequence is, 1st it has to be machined then welded and after that heat treatment upto 60 HRC.
I want to know the welding process and filler. in service this part has to bear a high pressure of flux.
Kindly guide me about welding and right filler material for this part.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...