Dear Sir,

Hi Friends please help me to clear the doubt

I have PQR qualification for 8mm thickness Fillet welding by using E6013 electrode. as per IS 7307 - Part I (1974).

Base material IS 2062 Grade B

Is it necessary to qualify 8mm thick by using E7018 electrode?
4. Changes affecting approval
4.1 A welding procedure test shall be required when any of the following changes are made to an approved welding procedure:

4.1.f ) Any change in type of electrode, filler material, flux or shielding gas.

As per IS 7310 Part I (1974)

5. Extent of approval
5.1 General - The extent of approval for a welding procedure. When a change in the welding procedure according to $ of IS 7307 (part I) - 1974 require a new welding procedure test, this shall entail re-approval of the welder except in the following cases :
c) A change from a basic to a rutile covered electrode.

Please help for a clear answer.

Thanking you for you valuable time you are going to give me in this case.

Dear Sir,





Thanking You.

With Warm Regards,

Muthu barathi P,
Mobile No. 9099006785

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...