[MW:15337] RE: 15332] MPT test method to check the Lamination on the Bevel Edge.

Dear Biplab

 

It depends on what type of defects you expect.

 

If it is surface defect then AC mode is sufficient.

 

If any near to surface defects are expected, then DC ( either HWDC or FWDC) can be used.

 

You may kindly refer to ASTM E1444 for the code reference.

 

Hope this helps.

 

Regards

Fredric Prabu. K

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Biplab Pal
Sent: 17 September 2012 19:36
To: materials-welding
Subject: [MW:15332] MPT test method to check the Lamination on the Bevel Edge.

 

Dear Exparts,

 

I have a doubt regarding MPT method.

I am going to check the lamination of plates from the bevel edges.

What MPT current mode should we use.

Is it AC or HWDC?

Please share your knowledge and code references.

 

--

Thanks & Regards
Biplab Pal
Welding Inspector

E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



The Message may contain confidential and/or privileged information. If you have received the message in error, please notify us immediately by responding to this email and then delete it from your system. In case of any further clarification you can contact us at info@itwindia.com and visit our website www.itwsignodeindia.co.in. Thank you for your cooperation.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...