Monday, September 17, 2012

[MW:15330] RE: 15323] Alloy Material Hardness

No

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Monday, September 17, 2012 2:14 AM
To: materials-welding@googlegroups.com
Cc: zakaria ghrab
Subject: [MW:15323] Alloy Material Hardness

 

Dear experts,

  We're going to construct a new power station; according ASME sect B31.1.

We have many alloy steels (Grades P11, P91, P22 material)  welded joints. Even when PWHT is performed, our client say that we don't have to perform hardness test.

Even NDE is the client scope, i'm searching for support from code to have exact infiormation, uis it mandatory ?

Need your help.

Regards.

--

زكرياء غراب
GHRAB Zakaria

Site QA/QC Manager
SDEM Entreprises

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...