Re: RE: [MW:14363] MOC for High H2S gas under pressure

Dear Mr. Vinod,
 
I agree with Mr. Goswami' reply. You can refer NACE MR-0103 & NACE MR-1075 for quality checks, corrosion allowance and Fabrication.
 
B.R.
 
C. R. GANDHI
(MANAGER- Q.A./ Q.C.)

--- On Fri, 5/25/12, manpreet <manpreetsin88@rediffmail.com> wrote:

From: manpreet <manpreetsin88@rediffmail.com>
Subject: Re: RE: [MW:14357] MOC for High H2S gas under pressure
To: materials-welding@googlegroups.com
Date: Friday, May 25, 2012, 1:02 PM

Hi,

If it was Oil & Gas Pipeline and ISO 15156' complaince was mandatory, SS316 wouldn't be allowed as per table A.2 of ISO 15156-3.

Regards,
Manpreet Singh



On Fri, 25 May 2012 04:53:37 +0530 wrote
>

Hi Vinod,



Generally austenitic stainless steels are very popular materials in

pharmaceutical industry due to hygiene and cleanliness issues. The selection

may vary from 304L 316L/LN and to the higher ends also.



Alternative could be duplex S.S also(see as attached).



The other options could be fluoro-polymers.But this is fairly new area in

terms of MOC.(seethe DuPont article)



I would think based on the operating parameters presented below a choice

between austenitic S.S or duplex could be ideal.



Thanks.



Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist

Ontario, Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net



-----Original Message-----

From: materials-welding@googlegroups.com

[mailto:materials-welding@googlegroups.com] On Behalf Of Aniket Gupta

Sent: Tuesday, May 22, 2012 4:13 AM

To: materials-welding@googlegroups.com

Subject: Re: [MW:14337] MOC for High H2S gas under pressure



You can use Carbon Steels with Nace Quality ( Controlled Composition of

Alloys).

Ex SA 516 60 ( Nace for Sulphide Cracking) Some of the clients want Heat

Treatment after fabrication.



Aniket Gupta



On 5/20/12, vnbhatt@gmail.com wrote:

> Respected Material Experts,

>

> We have a pharmaceutical client inquiry where they have gas media with

> 60 % H2S gas in the mix with 500 PPM moisture flowing from piping,

> vessels and shell-tube exchanger under pressure of 37 bar gauge.

>

> With many experienced brain on group, I seek details as to what MOC to

> be employed, what quality checks and what corrosion allowance??

>

> Appreciate guidance.

>

> Regards,

>

> Vinod Bhatt

> Sent on my BlackBerryR from Vodafone

>

> --

> To post to this group, send email to

> materials-welding@googlegroups.com

> To unsubscribe from this group, send email to

> materials-welding+unsubscribe@googlegroups.com

> For more options, visit this group's bolg at

> http://materials-welding.blogspot.com/

> The views expressed/exchnaged in this group are members personel views

> and meant for educational purposes only, Users must take their own

> decisions w.r.t. applicable code/standard/contract documents.

>



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to

materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at

http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and

meant for educational purposes only, Users must take their own decisions

w.r.t. applicable code/standard/contract documents.



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...