Dear Maganth,
 
I assume person from the TPI is good in technical.
 
Assume the product may be in the Jack case applications in Shipbuilding or similar applications.
 
In order to reduce the fabrication time , they will go for the forged rather than the 2 pcs then weld again.
 
In that cases, the best way to do welding simulation by welding the actual test pcs by approved WPS.
 
Majority of the cases, the forged company will supply small test pcs from the production heat for the verification to the customer approval
 
If the plate thickness is more than 100 mm , it is suggested to do verification of WPS in actual forged steel materials
 
Since the forged materials , may be less in CVN and elongation , it is better to verify the mechanical properties in the actual pcs after welding by approved WPS.
 

 
On Wed, May 30, 2012 at 1:00 PM, Lab <lab@cochinshipyard.com> wrote:
Dear Friends,
 
In our production unit, we would like to make butt weld between forged steel grade of S355J2G3, a round shaped object. The Third part Inspection (TPI) agency which clears the joint, insists us to perform WPS on similar material before production welding. This particular material was imported from other country long back and we could not thick about WPS when we purchased. It is not possible for us to get the similar material (same grade & same condition) suitable for WPS as well as WPQ and no response from the suppliers when contacted for supply of small quantity.
 
At last one supplier came forward and ready to supply S355J2G3 of rolled and normalized plate.
 
When we went to TPI with the proposal of making WPS with rolled plate, they are not convinced as the properties of forged and rolled steel even after Normalizing, are different and insisting us to do WPS test on forged steel of same grade.
 
Request the forum to provide guidelines to get rid of this situation or from where I get small quantity of material of similar grade, condition in India to arrange for WPS.
 
Regards,
Megnath
The information contained in this message are Cochin Shipyard Limited confidential and proprietary information and is intended only for the use of the recipient(s) named above. If the reader of this message is not the intended recipient, he/she is hereby notified that any use, dissemination, distribution, or copying of this communication or any of the content is strictly prohibited. In such case, please advise the sender immediately and delete it from your system. Further acknowledges that any views expressed in the message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Cochin Shipyard Limited.      ----------------------------------  Cochin Shipyard Ltd, Cochin, India      !-- Virus-Free Mail Using AntiVirus for PostMaster Enterprise & QuickHeal Engine --!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...