Re: [MW:14435] Uncertainity calculation in Tensile test

Dear Megnath,
                   Just follow ISO guide on Uncertainty Measurement. In simple steps:
1. Take atleast five readings for the required parameters (n=5)
2. Calculate, Mean & Standard Deviation
3. Take machine uncertainty given in calibration certificate
4. Combine and calculate Combined Uncertainty.

2012/5/31 Lab <lab@cochinshipyard.com>
Dear friends,
 
Can any one spare the Uncertainty Measurement of tensile test (Tensile strength, % Elongation etc) using UTM. This is just to understand before NABL Accreditation.
 
Regards,
A Megnath
The information contained in this message are Cochin Shipyard Limited confidential and proprietary information and is intended only for the use of the recipient(s) named above. If the reader of this message is not the intended recipient, he/she is hereby notified that any use, dissemination, distribution, or copying of this communication or any of the content is strictly prohibited. In such case, please advise the sender immediately and delete it from your system. Further acknowledges that any views expressed in the message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Cochin Shipyard Limited.      ----------------------------------  Cochin Shipyard Ltd, Cochin, India      !-- Virus-Free Mail Using AntiVirus for PostMaster Enterprise & QuickHeal Engine --!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...