Lower the Amperage, Higher the velocity.
Roy
Bohler Welding Group
-----原始邮件-----
From: bo gyi
Sent: Thursday, May 31, 2012 8:40 AM
To: Materials & Welding
Subject: [MW:14422] SS347 overlay but FN is too low
Dear all,
I have encountered that Ferrite No is too low for SS347 overlay to P1
(SAW).
I used ESAB ER309L & ER347 together with OK flux 10.93 and heat input
is about 0.9 - 1 kJ/mm.
My Ferrite no is as bellow . (check by Ferrite scope)
1st layer 309L (2mm thk from BM) , FN no. < 0.5
2nd layer 347 ( 4 mm thk from BM) , FN no < 2
3rd layer 347 ( 6 mm thk from BM) , FN no < 3.5
Required FN is 5 to 11 FN,
My welding parameters are as follow.
For 309L , 280 � 330 A, 30 � 32 V , travel speed 720 � 800 mm/min
For 347 , 330 � 350 A, 32 � 34 V , travel speed 720 � 800 mm/min
Please advice.
Regards,
Bogyi
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment