Remember you can't judge depth with a radiograph.
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vu Duc Thuan
Sent: Wednesday, May 30, 2012 1:38 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:14413] Code & Standard for Tubing
Dear All,
Thanks for your supporting,
that mean, we will check RT films and the densities of RT film to be measured at both weld metal and base metal location, it should compared the densities result as per B31.3 table 341.3.2
Regards,
Vu Duc Thuan
Email: dthuan117@gmail.com
Mobile: +84 983 017 936
Sky: vdthuan_vtau
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of sankar bombay
Sent: Wednesday, May 30, 2012 11:40 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14408] Code & Standard for Tubing
Dear friend,
B31.3 there have given teh acceptance for the root concavity check
table:341.3.2
check the density of the root and parrent material.. its should not
more than parent materialn at concavity side ( lenght is not given we dont
want to considered )
API 510 we have accpetance its should not be more 6mm lengh of
concavity
depth same
Regards
sankar.k
On 5/30/12, Vu Duc Thuan <dthuan117@gmail.com> wrote:
> Dear Expert,
>
>
>
> In my project, we have some tubing line ( ½" SS316L and Duplex) need
> to weld with reducer same material, we have WPS for both of material.
> The problem is the RT report show internal concavity but we do not
> have accept criteria for those weld joints as per drawing, Spec..etc..
>
>
>
> Kindly please advise which code & standard are using for the tubing. (
> tubing fix on the hydraulic control panel )
>
>
>
>
>
> Regards,
>
>
>
> Thuan
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
--
shankar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment