Dear friend,
B31.3 there have given teh acceptance for the root concavity
check table:341.3.2
check the density of the root and parrent material.. its should
not more than parent materialn at concavity side ( lenght is not given
we dont want to considered )
API 510 we have accpetance its should not be more 6mm lengh of concavity
depth same

Regards
sankar.k

On 5/30/12, Vu Duc Thuan <dthuan117@gmail.com> wrote:
> Dear Expert,
>
>
>
> In my project, we have some tubing line ( ½" SS316L and Duplex) need to
> weld
> with reducer same material, we have WPS for both of material. The problem
> is
> the RT report show internal concavity but we do not have accept criteria
> for
> those weld joints as per drawing, Spec..etc..
>
>
>
> Kindly please advise which code & standard are using for the tubing. (
> tubing fix on the hydraulic control panel )
>
>
>
>
>
> Regards,
>
>
>
> Thuan
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
shankar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...