Weld with a rutile flux electrode, the rutile will help minimize the
potential fro cracking caused by the Zinc.
To repair the galvanizing after welding use a Galvanizing Repair Rod
http://www.zaclon.com/pdf/alloy_repair_rods_data.pdf.
Richard
Original Message:
-----------------
From: Roy Liu standardliu@hotmail.com
Date: Tue, 29 May 2012 19:35:58 +0800
To: materials-welding@googlegroups.com
Subject: Re: [MW:14389] Welding Electrode for galvenised Iron(GI)
Brazing is the best way to weld such kind of material. otherwise the
Galvansied layer will be destroied.
Roy
Bohler Welding Group
From: shashi pandey
Sent: Monday, May 28, 2012 11:37 PM
To: materials-welding@googlegroups.com
Subject: [MW:14385] Welding Electrode for galvenised Iron(GI)
Dear Experts,
Can you please suggest me about best welding electrode for galvenised
Iron(GI) pipe/plate etc.?
What will be the effect on GI materials if it will be welded with MS/CS
welding electrode?
--
With Thanks....?
SHASHI B. PANDEY |SR. ENGINEER(MECHANICAL) |LANCO GROUP.
RAJNANDGAON, CHHATISHGARH | MOBILE: +91 8305357495
| Go Green | The future will thank you |
--------------------------------------
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--------------------------------------------------------------------
mail2web.com ā What can On Demand Business Solutions do for you?
http://link.mail2web.com/Business/SharePoint
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
potential fro cracking caused by the Zinc.
To repair the galvanizing after welding use a Galvanizing Repair Rod
http://www.zaclon.com/pdf/alloy_repair_rods_data.pdf.
Richard
Original Message:
-----------------
From: Roy Liu standardliu@hotmail.com
Date: Tue, 29 May 2012 19:35:58 +0800
To: materials-welding@googlegroups.com
Subject: Re: [MW:14389] Welding Electrode for galvenised Iron(GI)
Brazing is the best way to weld such kind of material. otherwise the
Galvansied layer will be destroied.
Roy
Bohler Welding Group
From: shashi pandey
Sent: Monday, May 28, 2012 11:37 PM
To: materials-welding@googlegroups.com
Subject: [MW:14385] Welding Electrode for galvenised Iron(GI)
Dear Experts,
Can you please suggest me about best welding electrode for galvenised
Iron(GI) pipe/plate etc.?
What will be the effect on GI materials if it will be welded with MS/CS
welding electrode?
--
With Thanks....?
SHASHI B. PANDEY |SR. ENGINEER(MECHANICAL) |LANCO GROUP.
RAJNANDGAON, CHHATISHGARH | MOBILE: +91 8305357495
| Go Green | The future will thank you |
--------------------------------------
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--------------------------------------------------------------------
mail2web.com ā What can On Demand Business Solutions do for you?
http://link.mail2web.com/Business/SharePoint
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments