Re: [MW:14389] Welding Electrode for galvenised Iron(GI)

Brazing is the best way to weld such kind of material. otherwise the Galvansied layer will be destroied.
 
  Roy
Bohler Welding Group
 
Sent: Monday, May 28, 2012 11:37 PM
Subject: [MW:14385] Welding Electrode for galvenised Iron(GI)
 
 
Dear Experts,
Can you please suggest me about best welding electrode for galvenised Iron(GI) pipe/plate etc.?
What will be the effect on GI materials if it will be welded with MS/CS welding electrode?
--

With Thanks....?

SHASHI B. PANDEY |SR. ENGINEER(MECHANICAL) |LANCO GROUP.

RAJNANDGAON, CHHATISHGARH | MOBILE: +91 8305357495

| Go Green | The future will thank you |

--------------------------------------


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...