Tuesday, May 29, 2012

Re: [MW:14387] equivalent ASTM material for DIN st52-3 Plate

Dear Asad


It can be useful for you.

Thanks& Regard's

Srinu.

On Mon, May 28, 2012 at 2:57 PM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings.
 
Please inform whether A 572 GR 50 plate is Equivalent to DIN st52-3 Plate.
 
Please provide me any comparision table for the materials.
 
Thanks & Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Srinu.B
QC Inspector
Harm Chang Day
Ras Al Khair Site (Desalination Project)
Ph:-+966536591968

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...