RE: [MW:14384] Range of approval for WELDER qualified to weld grove welds according to API 1104

Hi Malemela,

That depends on which Code is used, ASME Sec IX or API 1104. If ASME Sec IX, a welder qualifies groove weld also qualified to weld all fillet welds at the same time.

However, in API 1104 it's different, a welder who qualifies to weld V-groove allow to weld V-groove only. It is stated in API 1104 para. 5.4.2.3 that "A major change in joint design (for example, from V groove to U groove) constitutes an essential variable". A change from a butt to a fillet weld is a major change in joint design. That welder would therefore, not be qualified to make fillet welds.

I hope this helps.


From: smalemela@spc.co.za
To: materials-welding@googlegroups.com
Subject: [MW:14374] Range of approval for WELDER qualified to weld grove welds according to API 1104
Date: Mon, 28 May 2012 08:20:12 +0200

Hi Colleagues,

 

I am working on a pipeline construction project in Mpumalanga –South Africa. The client is a reputable water utility company in South Africa who has appointed a contractor to construct 37 km of 610mm Diameter pipeline. The joint design is Partial Joint Penetration ( by means of fillet weld). The pipe fit up is spigot and socket joint.

 

The appointed inspection authority is refusing to accept welder qualification for 'v' grove joint design allegedly because the client specification has asked for fillet weld and NOT butt weld.

 

Requalification of welders is not an issue apart from the time it will take to set up and get the qualification test done. I also know from training that range of approval for grove includes fillet welds as well.

 

Should I simply re-qualify the welders although their qualification covers fillet welds if range of approval is considered or should I insist on the inspection authority consulting for proper information on this matter?

 

The integrity of the profession is under threat if people without proper knowledge are allowed to rewrite the specifications for the industry and go unchallenged.

 

Your urgent response will be greatly appreciated.   

 

MALEMELA  N. S.

SITE MANAGER

SOUTHERN PIPELINE CONTRACTORS

6 Main Reef Road

DUNSWART

1508

TEL:0119148519

FAX:0119144524

CELL:0823892592

www.spc.co.za

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...