Dear peter paul,
                 
According to this, the welder should qualified above 2.5"(inch)O.D.... He should weld (qualified) upto unlimited outer dia of pipe.(O.D).But it should be differ from thickness of pipe.....
 
Thanks & Regards
M.Riyas

 
On Mon, May 28, 2012 at 5:15 AM, Peter Paul <paul@rigresources.com> wrote:

Dear Expert,

 

Please advise me (clear my doubt) if my 6G Welder can carry-out the work with the following info . My welder qualification is at 3.5" (OD)[WT=12.7mm]. While the actual work is 4"OD [WT=8.56 mm(Sch 80)].

 

I will allow my welder to carry-out welding with the concession of monitoring his progress by NDT-RT. How often do I take RT? (is it 10% of his weld joint as per BS and ASME std?) Please revert and advise. Thank you!

 

 

Respectfully yours,

Peter Paul

 

+65 9939 5904

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...