Re: [MW:14361] Time between root pass and hot pass

DEARS,
         Yes, u need to cut and reweld. Mostly hotpass is to burn and float out wagon track present in root pass ,so time between root and hot pass is 5 to 10 minutes


Regards,

SENBE

On Tue, May 15, 2012 at 5:25 PM, jesti fer <jesti_fer@yahoo.com> wrote:
Dear all,
We are doing 20" pipe line project with API 5L Gr.B material as per B31.4, Welding process SMAW (E6010 for root and rest with E 7018, both are up-hill) our welder welded one joint root pass and he kept this joint for long time. But our Qc instructed to cut and re-weld the joint. But the time between root pass and hot pass not mentioned in approved WPS and client specification also.
It necessary to cut and re-weld?
It is mentioned any were in the code (ASME or API)?
 
Please help me,,
  
Best Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...