Dear Mr. Park,
Figure 4.4-Positions of Test Pipe or Tubing for Groove Welds (see 4.2.4)
Figure 4.6-Positions of Test Pipes or Tubing for Fillet Welds (see 4.2.4)
--
George Xue (Xue Guoliang)
Tel: +86-512-68639769 Fax: +86-512-68639492
Email: cxueguoliang@gmail.com
Skype: xuegl2001
2012/5/24 Saravanan Sornam <saravanshyla@gmail.com>:
> Dear Mr.Park,
>
> Please refer and follow AWS D1.1 Table-4.1 and Table 4.5 for Essential
> Varaiables for Welding Position.
>
> For testting, you can refer clause 4.12 for tubular connections.
>
> Hope U can search all these from Section 4, AWS D1.1.
>
> FYI, I am working for KC Cottrell, Anseong city, Gyeonggi-do Korea.
>
> Cheers,
> SARAV.
> Anseong, Korea
> 010-7218-1706
>
>
>
> On Thu, May 24, 2012 at 7:16 AM, 박종민(PARK, JONG MIN) <carpediem@dsme.co.kr>
> wrote:
>>
>> Dear Experts
>>
>>
>>
>> WPS for 6GR could be developed via 6GR coupon in accordance with AWS D1.1.
>>
>> However, sample test or tubular mock-up test is required from time to
>> time.
>>
>>
>>
>> 1st question
>>
>> Are they mandatory for all 6GR qualification test?
>>
>> 2nd question
>>
>> Can fabricator select test method, sample test or tubular mock-up ?
>>
>>
>>
>> Your prompt advice would be highly appreciated.
>>
>>
>>
>>
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-