Wednesday, May 23, 2012

Re: [MW:14347] Connecting holes coming on butt joint area

You can drill the holes if they are inevitable to move from but strengthen the area of weld by any means.

Ammar

On Wed, May 23, 2012 at 7:21 PM, sreedhar ch <sdchitturi@gmail.com> wrote:
If shifting the hole is inevitable , then use(weld) a splice plate towards the Nut side  and drill through both plates.
 
rgds
Sreedhar

On Sun, May 6, 2012 at 8:38 AM, jaya anil <nethalaanil@gmail.com> wrote:
Dear Raju,

Generally Code wont specify this type of drilling on but joint, but if
there is no chance of shifting the hole from butjoint, you can drill
hole , if your weld joint is sound. and also if your hole size is
less.

regards
Anil Kumar
On 5/5/12, prabhakarmet@gmail.com <prabhakarmet@gmail.com> wrote:
> Dear Friends,
>
> I have one query. We are fabricating structures as per AWS D1.1.
> Connecting holes on web/flanges are coming exactly on the butt weld joint
> area.
>
> Can anyone tell me, whether drilled holes are allowed on butt joint areas?
> What does code specify in this regard?
>
> Thanks in advance.
> Regards,
> G.P.Raju
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS