Tuesday, May 22, 2012

Re: [MW:14342] Regarding Shell as per UG-80

Hi,

Mr patel As per code minimum of template will be ID/4 also
tabulate check in & check out values at various sections compare with
std chart in code.

Regards.

Manjunath.

On 5/21/12, Harry Patel <harryeng.09@gmail.com> wrote:
> Sirs,
>
> As per UG-80 When Internal pressure applicable, We have to check Shell
> ovality as per code.
> When External pressure applicable than Ovality and with the help of
> template circular form checking required.
>
> Client is asking for internal pressure also, with help of template
> checking required.If you know any clause in ASME let me know and let me
> know any thumb rule and minimum length of template
>
> Hope for your reply.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...