DEAR SIR,
 
PREQUALIFIED WPS GENERALLY USED FOR STATIC LOADING STRUCTURE ONLY WITH AN ALL ESSENTIAL VARIABLES ARE CARRIED OUT AS PER PREQUALIFICATION.GENERALLY IT WONT REQD FOR PQR QUALIFICATION BUT AS WELL BASED ON THE CLIENT APPROVAL TOO.
 
REGARDS
 
DINESH



On Mon, May 21, 2012 at 7:24 PM, samshuddin k <sam.renja@gmail.com> wrote:
Dear All

What is pre qualified WPS as per AWS D1.1

Its allows to write a WPS without PQR...?

Please explain

Regards

Samshuddin.K

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...