Dear experts,
Can any one answer the following: one inches butt weld is radiograped
double wall single image technique. The wall thickness is 2.91 mm and
weld reinforcemnt is 1.6mm. In accordance with ASME-V article-2 T-276
what will be the thickness that the penetrameter based on. In another
way the thickness that the penetrameter based on will be
(2.91mm+1.6mm=4.51mm) or (2.91 mm+2.91mm+1.6mm +1.6 mm=9.02mm) ?
The "interpretation" of ASME Section V clearly defines the "Material
thickness" in question.
The height of weld reinforcement at both sides of pipe is applicable
in this case &
which wire is be visible
Looking forward to have your answer with appreciation.
Many Thanks in advance
Regards
Pradip
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment