Have u done any electrode baking before use?
Welding parameters plz.
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of
murtaza506@yahoo.com
Sent: Tuesday, May 29, 2012 5:34 PM
To: Materials & Welding
Subject: [MW:14386] MMA welding Electrode Gets red hot
I have a MMA welding electrode of SS 308L Dia. 2.6mm. when half of
the electrode is consumed it get red hot, and it gives porosity in the
weld metal what could be the reason i.e. is it a welding problem or
there is a problem in the electrode???
if this problem is due to electrode then what can be the reasons and
rectifications???
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Welding parameters plz.
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of
murtaza506@yahoo.com
Sent: Tuesday, May 29, 2012 5:34 PM
To: Materials & Welding
Subject: [MW:14386] MMA welding Electrode Gets red hot
I have a MMA welding electrode of SS 308L Dia. 2.6mm. when half of
the electrode is consumed it get red hot, and it gives porosity in the
weld metal what could be the reason i.e. is it a welding problem or
there is a problem in the electrode???
if this problem is due to electrode then what can be the reasons and
rectifications???
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments