Tuesday, May 29, 2012

[MW:14391] RE: 14382] Hardfacing overlay on SA 572 GR 50 PLATE by IRON BASE RODS

You will probably find that a hard facing alloy does not fit any of the chemistry range requirements of QW-422.  However, QW-255.1, “Welding Variables Procedure Specifications (WPS) Gas Metal Arc Welding (GMAW and FCAW)” does not require an A number.  The classification or trade name of the filler metal (QW-404.12) is an essential variable.  Thus, for example, if your procedure qualification hardfacing filler metal was ConformaClad 700® , which is a proprietary alloy without classification, you may only perform the production overlay with Conforma Clad 700®.  If on the other hand you used Stellite 6® , classified as SFA/A .21 ERCCoCr-A, you could use any hard facing filler metal classified SFA/A .21 ERCCoCr-A.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Monday, May 28, 2012 9:15 AM
To: materials-welding@googlegroups.com
Subject: [MW:14382] Hardfacing overlay on SA 572 GR 50 PLATE by IRON BASE RODS

 

Dear All,

 

Greetings.

 

A hardfacing overlay has to be carried out on  A572 GR 50 Plate by FCAW - Semiautomatic Process as per ASME SEC IX.

 

rod used will be iron based.

 

please inform me what will be the SFA No. how we can decide A No.

 

Please give code reference.

 

Thanks & Regards

 

Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...