Tuesday, May 29, 2012

[MW:14388] Acid pickling necessity of Inconle 625 (overlay)

Dear experts

we are going to manufacturer a pressure vessel with A516-70 and overlayed by Inconle 625, overlay will be carried out by GMAW process, I want to know about necessity of Acid Pickling after overlay process. would you please share with me some technical/standard information in this regard.

Regards,
himan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.