Monday, May 28, 2012

[MW:14371] Re: 14365] HOW TO Calculating Electrode Consumption for Pipe Per Weld

a simple formula for you reference.
 
 
Roy
Bohler Welding Group
 
 
Sent: Monday, May 28, 2012 12:05 AM
Subject: Re: [MW:14365] HOW TO Calculating Electrode Consumption for Pipe Per Weld
 
http://www.t-put.com/english/634_ENG_HTML.htm

Magalhães Júlio

Welding and Inspection Around the world









2012/5/27 Asan Ibrahim <asan.ibrahim7@gmail.com>
Dear sir/mam


how to   Calculating Electrode Consumption for Pipe Per Weld. Is there is any formula reg to this kindly help me


REGARDS

R.ASAN
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to mailto:materials-welding%2Bunsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...