[MW:14339] Re: 14332] SAW consumable for welding 4130

They are T-PUT (Thyssen Former) brand's products.
But I think UV 420 TTR is enough.
 
 
Roy
 
Sent: Tuesday, May 22, 2012 8:54 AM
Subject: Re: [MW:14332] SAW consumable for welding 4130
 
Hi
 
Bohler Welding - Union S3 NIMO1(EF3) wire with UV 420 TTR-C flux gives better results.
 
Thanks
Regards
S.Eswaran
0065-96163449

--- On Mon, 21/5/12, Vikas Bhandari <vikas.bhandari349@gmail.com> wrote:

From: Vikas Bhandari <vikas.bhandari349@gmail.com>
Subject: [MW:14325] SAW consumable for welding 4130
To: materials-welding@googlegroups.com
Date: Monday, 21 May, 2012, 3:21 PM

Hi 
 
Can you please guide which consumable manufacturer' consumables are commonly used for welding low
alloy steel (AISI 4130, yield 520 MPa, Tensile 670 MPa, impacts at minus 30) with SAW process.
 
Thanks
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...