Hi,
As per Sec.V - T-224, it doesn't require to specify the weld thickness on the film. But As per T-290,weld thickness need to specify on the RT Reports. In your case you can accept the film and all other details shall be specified on the RT reports as per T-290.please find below the extraction of T-224 and T-290 for your reference.
T-224 System of Identification:
A system shall be used to produce permanent identification
on the radiograph traceable to the contract, component,
weld or weld seam, or part numbers, as appropriate. In
addition, the Manufacturer's symbol or name and the date
of the radiograph shall be plainly and permanently included
on the radiograph. This identification system does not necessarily
require that the information appear as radiographic
images. In any case, this information shall not obscure the
area of interest.
T-290 DOCUMENTATION:
T-291 Radiographic Technique Documentation
Details:
The Manufacturer shall prepare and document the radiographic
technique details. As a minimum, the following
information shall be provided.
(a) identification as required by T-224
(b) the dimensional map (if used) of marker placement
in accordance with T-275.3
(c) number of radiographs (exposures)
(d) X-ray voltage or isotope type used
(e) source size (F in T-274.1)
(f) base material type and thickness, weld thickness,
weld reinforcement thickness, as applicable
(g) source-to-object distance (D in T-274.1)
(h) distance from source side of object to film (d in
T-274.1)
(i) film manufacturer and Manufacturer's type/designation
(j) number of film in each film holder/cassette
(k) single- or double-wall exposure
(l) single- or double-wall viewing
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


From: Ramchandra vichare <vicharerke@indiatimes.com>
To: materials-welding@googlegroups.com
Sent: Thursday, December 22, 2011 5:59 PM
Subject: [MW:13257] Identification of thickness on Radiography films.

Dear Experts,

During Interpreting Radiography films at one of my vendor's works, I observed that, there is no identification /indicate thickness of job on film so I rejected the film. As far as generally everyone related field experience persons are know unless identification of thickness on film it is very difficult to know which penetrameter to be used but my vendor is arguing for the same. According to him one of "Level III" person insisit them there is no need to mentioned thickness in Radiography films and it sufficient if it indicate in Radiography interpretion report.
Suppose in piping number of joints/piping spools  are comming  with verious thickness in same report in such case it is possible to identify required penetrameter ? My anser is no, each Radiography films must be indicat thickness of joint/job.  Requested to suggest/advise.

Sincerely yours,
RK Vichare

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...