[MW:13292] Hydro testing failure

 
Dear friends,
 
During hydro testing of stainless steel, recently 2 tests leak occurred at welded joint area. I verified RT films, PMI reports...etc.Just I want to find root cause.
 
Please advise me that what proactive surveillance need to take of further hydro test failure & how it is happening..?
 
 
 
Thank you & Best Regards,

S. Dinesh Ravi Shankar.
Mechanical Inspector,
Saudi Aramco Project Inspection Division (SAPID),
Manifa Core Hydrocarbon Facilities Project.
Kingdom of Saudi Arabia.,
Mobile : +966 568059765,
Tel      : +966 3 379 2018.
 
  