Monday, October 31, 2011

Re: Re : [MW:12798] what filler metal can weld 1.4825

ER 309LSi(DCEN) FOR ROOT WELD

On Wed, Oct 26, 2011 at 6:06 PM, khemici badri <khemicib@yahoo.fr> wrote:
Hi;
 
I think that is better to use the  E308H-15 sticke lectrode (DCEP) to weld this grade in order to conserve a high temperature strength and creep resistance in the welded joint.
 
Regards
 
Badri
 

De : Roy LIU刘艺 <standardliu@hotmail.com>
À : materials-welding@googlegroups.com
Envoyé le : Mardi 25 Octobre 2011 14h11
Objet : [MW:12771] what filler metal can weld 1.4825

Hi, experts,

A furnace equipment wants to weld material 1.4825 (Material No.), which filler metals could be applied for this?


 
Best regards
 
Roy
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...