Hi Tarek
 
Please refer the following standard: BS 7570 - code of practice for validation of arc welding equipment.
After reading this standard you have to write your own company procedure and include in QA manual.
Visit our group's blog at http://materials-welding.blogspot.com/ wherin this same topic has been discussed in the past.
 
Regards
 
Prem S Nautiyal

Mobile     +91 9004063879 / 9769316004



--- On Mon, 10/31/11, Tarek Yehia <t.yehia2009@gmail.com> wrote:

From: Tarek Yehia <t.yehia2009@gmail.com>
Subject: [MW:12800] Welding Machines Calibration
To: materials-welding@googlegroups.com
Date: Monday, October 31, 2011, 6:22 PM

Dear Experts,

can any body tell me what is the recommended procedure for a/m subject and provide me with some written procedure or work instruction but should be based on applicable standard or suitable reference. 

--
Best regards,
 
Tarek Yehia


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...