Re: [MW:12793] If i have a WPS for 1G position groove weld (SAW) , Can i qualify lap joint welder ?

it can be qualified by grooved weld


On Sat, Oct 29, 2011 at 5:31 PM, tugrulhan özdemir <tugrulhan9@gmail.com> wrote:
Hi Welding People





I am little bit confused about an issue that can i qualify lap joint
with 1G groove weld wps or not? I could not found about what qualifies
lap joints. Can i consider lap joint as a filled weld and qualify by
groove weld?




Thank for your attention



Tugrulhan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...